Color: | White |
---|---|
Kind: | Processing Modifier |
Appearance: | Powder |
Still deciding? Get samples of US$ 0/g
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Haiflon® Polymer Processing Additives PPA9028F
ITEM | UNIT | Setting |
Bulk Density | g/cm³ | 0.6-0.8 |
Particle Size | mesh | <10 |
Active Ingredients | % | ≥97 |
Volatile | (105ºC1h)% | <1 |
The dispersion of PPA in resin determines the performance. The recommended process is to add PPA via 2%-3% Masterbatch through twin-screw extruder, and then add it into the extrusive resin according to the ultimate goal. The conditioning time is 20-60 minutes according to the equipment, base material and shear rate. No conditioning time when long-term use of this product.
Net weight 25kg per carton case